Carbon dioxide
1 - 7 of 7 results
|
Carbon dioxide is one of the global warming gases. Utilization of a sustainable energy is one of the effective technologies for the mitigation of CO2 accumulation in the atmosphere. If renewable energy can be used for methane synthesis, H2 is converted to methane by reducing CO2. We investigated the
Desalination 234 (2008)
|
|
Supercritical fluid extraction (SFE) of uranium and thorium from solid matrices was carried out employing CO2. Direct dissolution and extraction of oxides of uranium viz. UO2 and U3O8 was performed. UO2 and U3O8 powders (0.02–0.05 g) along with 2 ml of TBP–HNO3 complex were taken in extraction vesse
Desalination 232 (2008)
|
|
Whilst carbon dioxide is water soluble the system is somewhat complex and results in the presence of carbonate anions which interact with cations such as Ca2+ and Mg2+ present in seawater to form insoluble carbonates, especially at high temperatures. In multistage flash (MSF) desalination plants CO2
Desalination 220 (2008)
|
|
A new membrane material containing facilitated transport groups for carbon dioxide has been synthesized through the hydrolysis of polyvinylpyrrolidone (PVP) obtained by radical polymerization. The composite membrane was prepared with the hydrolysate as the top layer and microporous membrane as the s
Desalination 145 (2002)
|
|
As a new solvent free method for membrane formation, we have investigated the foaming of high-Tg polymers. We report two different routes for the formation of open-microcellular and open-nanoporous membrane morphologies. Porosity is introduced by expansion of carbon dioxide saturated films and hollo
Desalination 144 (2002)
|
|
This paper reports studies related to problems of vapour-side corrosion of copper/nickel alloys in multistage flash desalination plant. The main objective of the work was to obtain basic information and understanding of the corrosion behaviour of copper/nickel alloys in distilled water over a range
Desalination 138 (2001)
|
|
The paper describes a fundamental investigation of the corrosion behaviour of Cu-Ni-Fe-Mn alloys, containing nominally 10% Ni and 30% Ni, in distilled water. The study involved exposure of specimens to distilled water (1.5–7 µS/cm) at 20–80°C with and without injected carbon dioxide. At 20°C upon in
Desalination 126 (1999)
|